mysterymar mysterymar
I have used immersion, steaming and painting with acid dyes on wool roving. I'm diligent about following instructions, soaks, raising heat, tepid rinses, little handling, but the wool always ends up being almost felted. The strands are curly rather than straight like the commercial roving you buy. Is this expected? Is there something I can do to change the end result? I was told that it could be because commercial fibers are dyed before being combed. Is this true? I'm frustrated.
Thanks.
Reply 0 0
mysterymar mysterymar
Please help.
Reply 0 0
mysticalsister
Hi MysteryMar,
 
 I mostly dye cellulose fibers, but what this sounds like to me is that your fibers are combed tops. Combed tops, from what I understand, are so smooth and silky on the outside because they have been steamed and stretched (basically ironed) flat during the mill processing, which allows for very easy drafting.
 
However, as those of us with curly hair know, as soon as heat-flattened hair (or other mammal fibers such as wool) get exposed to humidity or outright liquid, all the frizz we just ironed out of our hair comes back with a vengeance. It’s impossible to avoid that unless the mill dyes the fibers _first_ and _then_ make it into combed top.
 
 This is one of the reasons why spinners should almost always wet finish any completed yarn *before* using it in a project. It’s essential to reactivate the curl in the fiber to see what the yarn is *really* like before trying to make a project and then having the project possibly get ruined the first time it encounters a humid environment or gets washed. A top that encounters moisture turns into not-top-anymore because the fibers disorganize themselves within the “noodle” - at that point, the top/sliver becomes a roving or semi-roving (depending on the natural crimp of the starting fiber. I could imagine a Lincoln or Wensleydale top - next to no crimp -  staying a top if careful avoidance of agitation is maintained)
 
 The felting on the outside is normal… to a certain extent. Part of that can be reduced by absolutely no stirring, moving, boiling, or other agitation of the fiber while it’s even slightly damp. Even just bending a damp roving slightly can cause felting in the outer layers. Another essential thing to avoid is any quick temperature changes. Even a shift from very hot water to less hot water or lukewarm to cool water can cause felting in the felting-worst-offender categories (pretty much anything that can felt from just compaction - if fiber artists use the phrase “____ felts if you just look at it wrong,” on the Internet, then that type of fiber is extremely felt-prone.
 
I hope this helps you or someone else like us here on the forum. Dyeing top/sliver/roving is especially difficult. Even many commercial products have felted outside surfaces (look at any review page for the spinning fiber “malabrigo nube” for the wide variety of felting complaints).
 
good luck - we need it!
Reply 1 0