Asterosperma
I’ve been using jacquard for around 15 years. Lately, I’ve been having issues with the ink cracking and peeling off the shirts. It no longer seems to pass the “stretch test”. I cure with a heat press for 1-2 mins at 275-300° depending on fabric and how thick  the deposit is. I’ve tried increasing the heat to 330° and then creasing the time but it doesn’t help. Has there  been a formula change? Is jacquard still able to cure with a thicker deposit? I use a 160-200 screen most of the time and put 2-3 thin layers down on dark shirts very quick flash (not enough to cure) between passes. It doesn’t happen with light tees and one pass.
Reply 0 0
Jacquardmod Jacquardmod
Thanks for getting back. I have done a lot of testing and I can't reproduce your results. Maybe the water is doing it. I have some Super Opaque white I want to send you that is a batch I tested thoroughly. I'd love to know if it still happens with this ink.  
 
I totally understand where you coming from. I am guessing something else is going on. I printed up to 8 layers and mixed different colors with it. I can't get it to crack even stretching a lot. Please email your address and phone number to techsupport@jacquardproducts.com and I will get some out to you.  
 
It's hard to think that you have continually gotten the same bad batch even if you are ordering from the same place. Please email me
Reply 1 0
Reply