TimChi
There is a fun video here about using Solarfast as a vat dye, but some details are missing.  So does anyone know if the powder added during the "dye bath" is soda?  And then what is in the "rinse bath", where the color develops.  I'd guess that its at least peroxide, maybe with some vinegar too?
 
Reply 0 0
Jacquardmod Jacquardmod
The soda is soda ash. Need a high pH for the chemical reaction.
 
I am not sure why we keep this up because it makes people want to do it, but you need sulfuric or nitric acid in the development bath.
 
I can share with you the procedure if you like, but I'd rather not post it here and send it directly to you via email. Contact me at techsupport@jacquardproducts.com if you want a copy of the procedure.
 
It isn't that crazy, just 1-2% strong acid in water, but having anyone go out and mess with strong acids seems a little dangerous to me.  
Reply 0 0
TimChi
Hey thanks for posting back!  I agree that strong acids need some care, along with strong alkali like NaOH, etc.  Its the adding of concentrated acid or base to water (or each other) were bad things can happen.  Always add acid to water; never add water to acid.
Reply 0 0
Reply